MIL-DTL-45301E
TABLE V. Classification and location of tests.
Title
Requirement
Tests
First article
Acceptance
First article
3.1
4.1.2
X
Tread elastomer
3.2.1
4.6.1
X
Tie gum
3.2.2
4.6.2
X
Backing
3.2.3
4.6.2
X
Vulcanization
3.2.4
4.6.3
X
Construction
3.3.1 thru 3.3.4 4.7.1 thru 4.7.4
X
Classes & sizes
3.4.1 thru 3.4.6 4.8
X
Physical properties
3.5.1
4.9.1.1
Hardness
3.5.1
4.9.1.1
X
X
Tensile strength
3.5.1
4.9.1.1
X
X
Elongation
3.5.1
4.9.1.1
X
X
Modulus
3.5.1
4.9.1.1
X
X
Specific gravity
3.5.1
4.9.1.1
X
X
Mooney viscometer
3.5.1
4.9.1.1
X/*
X
before aging
Ozone resistance
3.5.1 & 3.7.3
4.9.1.1 & 4.11.3
X
Low temperature
3.5.1 & 3.7.4
4.9.1.1 & 4.11.4
X
flexibility
Adhesion
3.5.3
4.9.1.2
X/*
Resistance to blowout
3.5.4
4.9.1.3
*
Resistance to separation 3.5.5
4.9.1.4
*
Storage life;
Classes 1, 2, 3 & 5
3.6.1.1
4.10.1.1
X
Classes 4 & 6
3.6.1.2
4.10.1.2
X
Workmanship
3.6.2
4.10.2
Mooney viscometer;
Accelerated aging,
3.7.1
4.11.1
X/*
classes 1, 2, 3 & 5
Accelerated aging,
3.7.2
4.11.2
X/*
classes 4 & 6
4.1.3 Conformance inspection.
4.1.3.1 Sampling.
4.1.3.2 Lot formation. Unless otherwise specified (see 6.2), a lot shall consist of not
more than 300 pieces, 300 rolls, or 5000 lb (2270 kg) from an identifiable production period,
11